Short answer: For steel parts that are galvanized after fabrication, such as fence posts, sign posts, grating and frames, specify ASTM A123 for US projects or ISO 1461 for most other markets. Use ASTM A153 for bolts, nuts and small hardware, and ASTM A653 for sheet that is galvanized on a continuous line before fabrication, with a coating designation such as G90 (0.90 oz/ft² on both sides combined). Minimum coating thickness rises with steel thickness: ISO 1461 asks for a 55 µm mean on 1.5–3 mm steel and 85 µm on steel over 6 mm.
Last updated: November 26, 2026.
This guide is for importers, brand owners and specifiers who buy galvanized steel products from overseas factories and need one clear line on the purchase order. It explains which standard covers which product, the minimum thickness each one sets, and how to check it at inspection. For choosing between zinc and stainless steel in the first place, see galvanized vs. stainless steel for outdoor products.
Batch galvanizing and pre-galvanized sheet are different products
Two processes both get called “galvanized”, and they are covered by different standards. In batch hot-dip galvanizing, the finished part is dipped in molten zinc, so welds, cut edges and the inside of tubes are coated. In continuous galvanizing, steel coil runs through a zinc bath before it is cut and formed. The American Galvanizers Association (AGA) notes that continuous coatings are nearly pure zinc and can be formed without cracking, while batch coatings are zinc-iron alloy layers bonded to the steel, which makes them more resistant to abrasion.
| Item | Batch hot-dip galvanizing | Continuous (pre-galvanized) sheet |
|---|---|---|
| When zinc is applied | After cutting, bending and welding | On the coil, before fabrication |
| Main standards | ASTM A123, ASTM A153 (hardware), ISO 1461 | ASTM A653 |
| How thickness is stated | Minimum per surface, by steel thickness | Designation for both sides combined, such as G60 or G90 |
| Cut edges and welds | Coated in the same dip | Left with little or no zinc; usually painted or powder coated |
| Typical products | Posts, grating, frames, brackets | Mailbox bodies, enclosures, panels |

ASTM A123: minimum coating by material category
ASTM A123 covers individual steel pieces and assemblies that are galvanized after fabrication. It sets a minimum average coating thickness that depends on the material category and the steel thickness. The AGA stresses that these are minimums only: the standard has no maximum thickness. Values below are in micrometers (µm); 45 µm is about 1.8 mils and 100 µm about 3.9 mils.
| Material category | <1.6 mm | 1.6–3.2 mm | 3.2–4.8 mm | 4.8–6.4 mm | 6.4–16 mm | >16 mm |
|---|---|---|---|---|---|---|
| Structural shapes | 45 | 65 | 75 | 75 | 100 | 100 |
| Strip and bar | 45 | 65 | 75 | 75 | 75 | 100 |
| Plate | 45 | 65 | 75 | 75 | 75 | 100 |
| Pipe and tubing | 45 | 45 | 75 | 75 | 75 | 75 |
| Wire | 35 | 50 | 60 | 65 | 80 | 80 |
A single fabricated part can contain several categories, for example tube welded to plate. Name the standard, not a single thickness, on the order, and let each component meet its own row.
ISO 1461: mean and local thickness
ISO 1461 is the general galvanizing standard used in Europe, the UK and many other markets. The current edition is EN ISO 1461:2022, according to the Wedge Galvanizing datasheet. It does not use material categories. Instead it sets a minimum mean thickness for a reference area and a lower minimum for any single local reading.
| Article (not centrifuged) | Local minimum | Mean minimum |
|---|---|---|
| Steel over 6 mm | 70 µm | 85 µm |
| Steel over 3 mm up to 6 mm | 55 µm | 70 µm |
| Steel 1.5 mm up to 3 mm | 45 µm | 55 µm |
| Steel under 1.5 mm | 35 µm | 45 µm |
| Castings 6 mm and over | 70 µm | 80 µm |
| Castings under 6 mm | 60 µm | 70 µm |
Small parts such as bolts are spun in a centrifuge after dipping to remove excess zinc, and they have lower limits: for threaded articles over 6 mm diameter, 40 µm local and 50 µm mean. The AGA comparison describes the two standards as very similar, with ASTM A123 typically requiring a little more thickness on most steel types.
Hardware and fasteners: ASTM A153
Bolts, nuts, washers, castings and other hardware fall under ASTM A153, which also covers embrittlement concerns for high-strength fasteners. If your fence or sign post kit ships with fixings, list A153 for the hardware next to A123 for the posts, so both are inspected.

Sheet products: what G60 and G90 mean
Under ASTM A653, a designation such as G90 states the coating weight on both sides of the sheet together. The AGA explains that G90 is 0.90 oz/ft² in total, or 0.45 oz/ft² per side, about 18 µm per side; the GalvInfo Center gives a similar estimate of about 21 µm per side and pairs G90 with the metric designation Z275 (275 g/m²). That is much less zinc per surface than batch-galvanized parts of the same thickness, which is why sheet-metal products such as mailboxes and enclosures are usually powder coated over the zinc.
| Designation (A653) | Total, both sides | Metric equivalent |
|---|---|---|
| G60 | 0.60 oz/ft² | — |
| G90 | 0.90 oz/ft² | Z275 (275 g/m²) |
| G115 | 1.15 oz/ft² | — |
What to write on the purchase order
- The standard and edition for each part: ASTM A123, ASTM A153 or ISO 1461 for parts galvanized after fabrication; ASTM A653 plus a designation such as G90 for pre-galvanized sheet.
- The steel thickness of each component, so the correct minimum applies.
- Whether the zinc will be painted or powder coated afterwards, so the galvanizer and painter can plan surface preparation.
- How thickness will be measured and reported. ISO 1461 calls for five or more readings at widely dispersed points on each reference area.
- How damaged areas may be repaired. ASTM A780 covers touch-up with zinc-based solder, zinc-rich paint or metallizing.
- Venting and drainage holes on closed sections, following the design practice in ASTM A385, so zinc can flow in and out of tubes.

Worked example: a fence post and a mailbox
A 2 mm square steel tube post that is galvanized after welding its base plate falls under ASTM A123 “pipe and tubing” for 1.6–3.2 mm steel, so the minimum is 45 µm; under ISO 1461 the same post needs a 55 µm mean and 45 µm local. A mailbox body bent from 1 mm sheet is different: if it is made from G90 pre-galvanized sheet, each face carries roughly 18–21 µm of zinc and the cut edges carry almost none, so the powder coat does most of the protecting. If the buyer needs batch galvanizing after fabrication instead, ISO 1461 asks for a 45 µm mean on steel under 1.5 mm, but thin sheet can warp in the bath, which the AGA also notes.
Galvanized products from HD Mechanical Vietnam
HD Mechanical Vietnam makes square sign posts and U-channel posts in hot-dip galvanized steel, steel grating with hot-dip galvanized finish, and galvanized steel posts for wood fences. Galvanizing is supplied to the standard named on your purchase order; agree the standard, the measurement method and the inspection report before production. Our quality documents guide lists what to ask for.
Frequently asked questions
What is the difference between ASTM A123 and ISO 1461?
Both cover steel galvanized after fabrication. ASTM A123 sets minimum average thickness by material category and steel thickness, while ISO 1461 sets mean and local minimums by steel thickness only; the AGA notes that A123 typically requires slightly more zinc.
Is G90 the same as hot-dip galvanizing?
No. G90 is a coating designation in ASTM A653 for sheet galvanized on a continuous line, meaning 0.90 oz/ft² on both sides combined, or roughly 18–21 µm per side. Parts galvanized after fabrication are covered by ASTM A123 or ISO 1461.
Which standard covers galvanized bolts and nuts?
ASTM A153 covers hot-dip galvanized hardware such as bolts, nuts, washers and castings. ISO 1461 also has lower limits for centrifuged threaded articles, for example 50 µm mean on threads over 6 mm diameter.
How is galvanized coating thickness checked?
Thickness is usually measured with a magnetic coating thickness gauge. ISO 1461 calls for five or more readings at widely dispersed points on each reference area, and the results should be compared with the minimums for each steel thickness.
How are damaged galvanized areas repaired?
ASTM A780 sets the practice for repairing damaged or uncoated areas, using zinc-based solder, zinc-rich paint or metallizing. Agree the allowed repair method and maximum repair area with your supplier before production.
Sources
- ASTM A123 for Structural Steel Products – American Galvanizers Association
- ISO 1461 vs. ASTM A123 – American Galvanizers Association
- ASTM Specifications (A153, A385, A780) – American Galvanizers Association
- ASTM A123 and G90 Specifications – American Galvanizers Association
- Hot Dip Galvanizing to EN ISO 1461 (datasheet, 2024) – Wedge Galvanizing
- GalvInfoNote 1.1: Metallic-Coated Products and Specifications – GalvInfo Center
Request a galvanized steel quote
Send your drawings, steel thickness, quantities and the galvanizing standard you need through our contact page or WhatsApp +84 98 878 53 93. See also how to write an RFQ for custom metal fabrication.